Aug 24, 2026

Key process parameters for ABS injection molding

Leave a message

Properties Explanation
Composition Trifunctional copolymer of acrylonitrile (A), butadiene (B), and styrene (S)
Mechanical properties High strength and toughness, good impact resistance
Processing properties Stable shrinkage rate, moderate melt viscosity, good fluidity
Temperature resistance range General operating temperature: -20℃ to 80℃
Chemical resistance Resistant to water, acids, and alkalis, but not resistant to strong oxidants and ketone solvents
Surface quality Good gloss after demolding, reducing the cost of secondary processing

 

Key process parameters for ABS injection molding
Table
Parameters Recommended Range Explanation
Melt Temperature 210–250℃ Adjust according to specific brand
Mold Temperature 30–120℃ Influences surface quality and internal stress
Injection Pressure 50–200 MPa Adjusted based on product complexity
Hold Pressure 30–150 MPa Prevents shrinkage
Clamping Force 30T–hundreds of tons Depends on the projected area of the product
Cooling Time Depends on wall thickness Ensures complete curing
Size Precision Up to ±0.02mm High-precision molds can reach ±0.01mm

Send Inquiry